Abstract
Superelso 890 (minimum yield strength of 890 MPa, or 130 ksi) is a high yield strength quenched and tempered steel alloy. This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code: SA-640. Producer or source: Industeel USA, LLC.