Abstract
ATI 64-MIL Titanium Alloy is a widely used alpha + beta titanium alloy with modifications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ti-148. Producer or source: ATI Defense.
This content is only available as a PDF.
Copyright © ASM International® 2011
2011
ASM International
You do not currently have access to this content.