Abstract

Sandvik Bioline 11R51 HV is the vacuum remelted version of the alloy required for higher cleanliness. This datasheet provides information on composition, physical properties, elasticity, and shear and bend strength It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SS-1100. Producer or source: Sandvik Materials Technology.