Abstract

Wieland-FX9 is a high-manganese bronze alloy that has good strength and is available in numerous cold work tempers related to its minimum tensile strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Cu-801. Producer or source: Wieland Metals Inc..