Abstract

DICREST is a series of fine grained pressure vessel steels with resistance to hydrogen induced cracking (HIC). This datasheet provides information on and physical properties. It also includes information on forming, heat treating, and joining. Filing Code: SA-629. Producer or source: Dillinger Hütte GTS.