Abstract

Crucible CPM 35VN was developed as an improvement over CPM S30V (see Alloy Digest SS-891, September 2003) and offers improved toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion and wear resistance as well as heat treating and machining. Filing Code: SS-1093. Producer or source: Crucible Industries LLC.