SSAB API GRADE 2MT1 is an intermediate strength steel alloy for steel plates at thicknesses through 63.5 mm (2.500 in.) for use in welded construction of offshore structures. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: SA-627. Producer or source: SSAB Swedish Steel Inc..