Abstract
Maxival MVAPMLD2 is an enhanced machining version of AISI Type 316L stainless steel. The alloy has a specified inclusion picture to enhance machining by modifying both sulfide and oxide inclusions. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming and machining. Filing Code: SS-1087. Producer or source: Valbruna Stainless Inc..