Abstract
FORA 450 is a wear resistant steel with a minimum HB hardness of 450. This water quenched martensitic steel is used in truck bodies. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on wear resistance as well as forming, machining, and joining. Filing Code: SA-624. Producer or source: Industeel Belgium.