Abstract

Ansonia alloy C35300 is a high lead content brass that fulfills the need for a strong brass with good machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-796. Producer or source: Ansonia Copper & Brass.