Carpenter Touralloy 230 Plus stainless was originally developed for high-strength aerospace components, however, it may provide improved bar cycle fatigue durability, compared to other traditional golf face plate alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1084. Producer or source: Carpenter Specialty Alloys.