Abstract

Creusabro Dual is an advanced development in wear-resistant steels where the metal, alloyed with 0.6% Ti, produces excellent sliding wear resistance. It is unique to offer wear resistance at this level of hardness (500 HB), with such high abrasion resistance combined with high resistance to cracking in service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on wear resistance as well as forming and joining. Filing Code: SA-639. Producer or source: Industeel USA, LLC.