Sandvik Bioline F562/F562L Ti are nonmagnetic nickel-cobalt base alloys with ultra high strength and great corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: Ni-693. Producer or source: Sandvik Steel Company.