Supralsim 690 is high yield strength steel for welded and weight-saving structures. This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming and joining. Filing Code: SA-637. Producer or source: Industeel USA, LLC.