Kubota Alloy HU is an iron-chromium-nickel alloy with moderate elevated temperature strength and good oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on casting and joining. Filing Code: SS-1105. Producer or source: Kubota Metal Corporation, Fahramet Division.