Abstract

NAS 8R10 is an austenitic stainless with a boron addition to provide shielding for uses in nuclear reactors. Storage racks is one application. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: SS-1081. Producer or source: Nippon Yakin Kogyo Company Ltd.