Abstract
Wieland-K11 is a pure, oxygen-free copper for many electronic and glass sealing applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Cu-794. Producer or source: Wieland Metals Inc., Wieland-Werke AG.