ENDURO HCN is an austenitic, non-magnetic chromium-nickel stainless steel having high creep and oxidation resistance at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SS-59. Producer or source: Republic Steel Corporation.