Abstract

CHAMET BRONZE is a copper-zinc alloy containing 0.75% of tin, having high strength, toughness and resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-50. Producer or source: Chase Brass & Copper Company Inc..