Abstract

DYNALLOY is a versatile low-alloy, high-strength, flat rolled steel which combines high physical properties with ductility and weldability. It has higher atmospheric corrosion resistance, and also higher resistance to abrasion, impact and fatigue than plain carbon steels. This datasheet provides information on composition, tensile properties, and bend strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-56. Producer or source: Alan Wood Steel Company.