Abstract

MST Grae III is commercially pure, unalloyed titanium made by the Method S melting process, offering improved weldability and impact strength This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-11. Producer or source: Mallory-Sharon Titanium Corporation.