BOHNALITE-Y is a heat treatable aluminum casting alloy recommended for high temperature applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-60. Producer or source: Bohn Aluminum & Brass Corporation.