Abstract

Ampcoloy 88 was developed for plastic tooling and has a hardness greater than 260 HB, a high thermal conductivity, with good machinability and polishability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: CU-787. Producer or source: AMPCO Engineered Alloys.