Docol W steels are weather resistant during outdoor use. These steels are designated according to their lowest yield strength. In addition to its weather-resistance properties, Docol W steels are characterized by high resistance to impact and wear, good formability, and weldability. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SA-616. Producer or source: SSAB Swedish Steel Inc.