Abstract

303 Ugima HD is the lower-sulfur version of Ugitech’s improved machining 303 grade. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1053. Producer or source: Schmolz + Bickenbach USA Inc.