Kubota Alloy HI is a heat-resistant stainless steel casting suitable for long-term service at temperatures up to 1105 deg C (2025 deg F). Furnace skids and rail, conveyor roll assemblies, lead pots and retorts are typical applications. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on corrosion resistance as well as casting and joining. Filing Code: SS-1052. Producer or source: Kubota Metal Corporation, Fahramet Division.