Luvata C50715 is a very common and frequently used alloy. The 2% Sn and coherent precipitates improve properties. It is often called CuSn2Fe0.1P. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. and bend strength. It also includes information on forming. Filing Code: CU-779. Producer or source: Luvata Sales (USA) Inc.