Abstract

HPM MP35N-LTi is a nonmagnetic nickel-cobalt-chromium-molybdenum alloy that has excellent corrosion resistance, can obtain ultrahigh tensile strengths 2068 MPa (300 ksi) through work hardening and aging, and has good toughness and ductility. Applications include electrical components, springs, and instrument parts in medical, chemical, food processing and marine environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: CO-120. Producer or source: Hamilton Precision Metals.