Abstract

Thermodur 2714 is a tough die steel with high tempering resistance and good through hardening. Typical applications include forging dies, mandrels, die holders, armored trim dies, and hot-shear blades. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming and heat treating. Filing Code: TS-694. Producer or source: Schmolz + Bickenbach USA Inc.