Electralloy F44 is a solution strengthened, austenitic stainless steel alloy with 6% Mo providing excellent resistance to aqueous corrosion, coupled with good strength and great pitting resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1077. Producer or source: Electralloy, a Division of G.O. Carlson Inc.