Abstract

Kaiser Alloy 6041 is a lead-free alternative to 6262 with good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming and machining. Filing Code: AL-432. Producer or source: Kaiser Aluminum. See also Alloy Digest Al-449, December 2016.