Sumitomo HN6SI is a high-temperature nickel-base alloy. The alloy exhibits resistance to both carburization and metal dusting. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming and joining. Filing Code: Ni-677. Producer or source: Sumitomo Metal USA Corporation.