Abstract

Kanthal APM HP is an advanced high-purity powder metallurgical dispersion-strengthened resistance heating or high-temperature alloy of the family FeCrAlMo that has good form stability at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming and powder metal forms. Filing Code: SS-1038. Producer or source: Kanthal AB.