OvaX 600 is an ingot cast through-hardening steel that is specially designed for air hardening or gas quenching and for applications requiring isotropic properties and very high cleanliness levels. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on casting, forming, and heat treating. Filing Code: SA-604. Producer or source: Ovako North America Inc.