Abstract
Domex 700MC is a high-strength low-alloy (HSLA) steel for cold forming operations. It is available in thicknesses of 2.00-10.00 mm. The alloy has a minimum yield strength of 700 MPa. Domex 700 MC with designation D and E meet and exceed the demands for steel S700 MC in EN-10149-2 for impact energy at low temperatures. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-602. Producer or source: SSAB Swedish Steel Inc. and SSAB Tunnplat AB.