Abstract

ATI 720 is a nickel-base alloy, solid solution strengthened with tungsten and molybdenum and precipitation hardened with titanium and aluminum. The alloy combines high strength with metallurgical stability as demonstrated by excellent impact strength retention after long exposures at elevated temperatures. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-669. Producer or source: Allvac, An Allegheny Technologies Company.