Abstract

ATI S240 alloy is a high-strength precipitation-hardening alloy with advantages in simple thermal mechanical processing, corrosion resistance, and lower costs than similar-strength alloys. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: SS-1035. Producer or source: ATI Allvac.