Abstract

Domex 650MC is a high-strength low-alloy (HSLA) steel for cold forming operations. It is available in thicknesses of 2.00-10.00 mm. The alloy has a minimum yield strength of 650 MPa. Domex 650 MC with designation D and E meet or exceed the demands for steel S650MC in EN-10149-2 for impact energy at low temperatures. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-599. Producer or source: SSAB Swedish Steel Inc. and SSAB Tunnplat AB.