Abstract
ElektronWE54 is fully heat treatable for use to 300 deg C (570 deg F) and is free of silver and thorium. The alloy is used in military and motorsport applications where these properties are at a premium. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: MG-77. Producer or source: Magnesium Elektron Wrought Products, North America.
cast magnesium alloys, castability, chemical composition, compressive strength, corrosion-resistant alloys, elasticity, Elektron WE54, fracture toughness, hardness, heat treatability, joinability, machinability, military applications, motorsport applications, physical properties, shear strength, tensile properties, thermal properties, UNS M18410
Copyright © ASM International® 2009
2009
ASM International
Topics
Corrosion-resistant alloys
Cast magnesium alloys
Magnesium alloys
Chemical composition
Castability
Heat treatability
Joinability
Machinability
Compressive strength
Elastic modulus
Fracture toughness
Hardness
Shear strength
Tensile properties
Physical properties
Thermal properties
Sports and recreation equipment
You do not currently have access to this content.