Alcoa alloy 6022 was developed for automotive closure panels and has higher strength and improved formability than other alloys. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: AL-421. Producer or source: Alcoa.