Abstract

LSS HW-108 is a hot work tool steel and an addition to the H10 chemistry group that provides increased resistance to softening at elevated temperatures. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating and machining. Filing Code: TS-678. Producer or source: Latrobe Specialty Steel Company.