Ansonia alloy C65100 is often called low silicon bronze and is used in aircraft hydraulic lines, various screws, and as pole line hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: CU-766. Producer or source: Ansonia Copper & Brass Inc.