Abstract

Alcan 6061 alloy in the annealed and aged tempers is a popular alloy. It possesses good mechanical strength and corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, machining, and joining. Filing Code: AL-427. Producer or source: Alcan Inc.