Abstract
DMV 931 is an alloy for general and chloride corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1047. Producer or source: Mannesmann DMV Stainless USA Inc.