ATI 600-MIL Ultra High Hard is a specialty steel of wrought Ni-Cr-Mo steel for armor plate. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-610. Producer or source: ATI Defense.