Ovako 253 is steel developed primarily for carburizing. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming and heat treating. Filing Code: SA-609. Producer or source: Ovako North America Inc. and Ovako Holdings AB.