Micro-Melt 420-CW is a powder-produced wear-resistant tool steel with corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on corrosion and wear resistance as well as forming, heat treating, machining, and powder metal forms. Filing Code: TS-676. Producer or source: Carpenter Powder Products.