URANUS 76N contains high chromium, molybdenum, and nitrogen contents and has a pitting resistance equivalent number (PREN) ≥ 40. These factors explain why the duplex austenitic/ferritic stainless grade is very resistant to localized corrosion. The alloy has been used for offshore applications. This datasheet provides information on composition, physical properties, tensile properties, and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1028. Producer or source: Industeel USA, LLC.