Abstract

Kubota UCX was developed for very high temperature operation for ethylene pyrolysis service. The alloy also has excellent oxidation and corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as casting and joining. Filing Code: Ni-663. Producer or source: Kubota Metal Corporation, Fahramet Division.