Luvata C1453 (CuTe0.02Sn0.02) is a copper tellurium alloy for electrical and heat-transfer applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on forming, heat treating, machining, and joining. Filing Code: CU-755. Producer or source: Luvata Sales (USA) Inc.